Edge Solutions

CDS — Clinker Detection System + ITM Connect

“Hear the clinkers fall — quantify fouling shedding before it damages the floor.”

CDS — Clinker Detection System

  • Records every clinker that hits the boiler floor: when it landed, which floor zone it hit and how big it was.
  • Ties each impact to the sootblower that was running when the deposit let go, so every sootblower has a measured count of clinkers per blow.
  • Shows where the superheater is fouling, from which sootblowers shed the most.
  • Tracks a chill-and-blow as it happens, and shows when the shedding has stopped.
  • Gives the same measure for other cleaning methods, such as sonic horns and pulse-detonation cleaning.
  • Built on ITM’s patented method — US 10,060,688 B2.
CDS in 42 seconds.

CDS — Clinker Detection App

Deposits build on the superheater until a sootblower, or a chill-and-blow, knocks them off. The large ones slide down the nose arch or fall straight from the tubes and hit the boiler floor, and nobody in the control room sees them land. CDS listens to the floor. Accelerometers on the floor’s supporting structure record each impact. Running on ITM Connect at the edge, the Clinker Detection App sizes the impact, places it in a floor zone, and ties it to the sootblower that was running. One measurement answers three questions: what hit the floor, which sootblowers are removing deposit, and whether a chill-and-blow is still shedding.

The CDS app on ITM Connect during a chill-and-blow: tiles for impacts in the last 30 minutes, the largest impact, red-band impacts, shed rate, the sootblower running and time since liquor off; a chart of impacts per hour rising to a peak and falling to a marked point where shedding stopped; a floor map of six zones with impacts as dots; clinkers per blow for twelve sootblowers with two marked to run more; a list of the largest impacts; impacts by size band; and the advisory bits sent to the DCS.
The CDS app on ITM Connect during a chill-and-blow. Concept screen with simulated data.
  • Every impact, recorded — time, floor zone and size for each impact above the recording threshold.
  • Size, in bands — each impact is reported as an equivalent weight and sorted into bands agreed for that boiler’s floor.
  • Large-impact alarm — an impact in the upper bands raises an advisory bit at the moment it happens.
  • Clinkers per blow — impacts are counted against the sootblower that was running, with the travel time down the nose arch allowed for.
  • Shed rate — impacts per hour through a chill-and-blow, with a flag when the rate stays below a set level.
  • Publishes it to the mill — the alarm, the shed rate and the sootblower figures go to the DCS, the sootblowing system and the historian.

At a glance: Accelerometers on the floor’s supporting structure · the floor divided into zones · size reported as equivalent weight at 30 m · three size bands · every impact tied to a sootblower · impacts per hour through a chill-and-blow · advisory beside the boiler’s own alarms.

Measuring at the floor is the differentiator. Other fouling measurements look at what is on the tubes. CDS measures what comes off them, at the moment it lands. The system is calibrated on the boiler itself: known weights are dropped from the access ports below the nose arch onto the bare floor during an outage, and the response of each sensor is recorded with the zone each weight lands in. The floor is divided into zones because it does not answer the same everywhere: floor tubes are stiffer near the walls than in the middle. After that, an impact is reported as an equivalent weight falling 30 meters, about 100 feet. It is a relative size and not a weighing, and it is enough to tell a nuisance from a clinker that can deform a floor tube.

An accelerometer signal from a calibration drop: flat, then a sharp burst of about 20 g that rings down over a few tenths of a second.
One calibration drop, as a floor accelerometer recorded it. From ITM’s ICRC 2017 presentation.

Why falling clinkers matter

Clinkers are the masses of ash deposit that form around superheater tubes. Some reach the size of a small car, and they can fall up to 150 feet before they hit the floor. The larger a deposit grows before it comes off, the harder it lands. A boiler with a history of floor-tube damage faces unplanned tube replacements at outages, and a damaged floor tube raises the exposure to a smelt-water explosion.

Operators have two tools against deposits: sootblowing and the chill-and-blow. Both are run without a direct measure of what they remove. A sootblower that runs is assumed to be a sootblower that cleans, and a chill-and-blow is ended on judgment, because there has been no way to know when the shedding is over.

The floor of a recovery boiler during an outage, with a row of floor tubes bent out of line where deposits have landed.
Floor tubes damaged by falling deposits
Diagram of a boiler superheater above a floor, with four numbered labels: clinker location, active sootblowers, falling clinker and boiler floor.
Where the deposit forms, the sootblower that removes it, the fall, and the floor

One floor. Three answers.

The same impact record serves the operator, the sootblowing strategy and the outage plan. A count of what each sootblower knocks down needs no model of the boiler, and it rests on one measurement that can be checked: something hit the floor, here, at this time.

A floor map of six zones from the front wall to under the nose arch, with impacts shown as dots coloured by size band; most land under the nose arch and one large impact is marked in red.

What hit the floor

Every impact large enough to matter is recorded with its time, its floor zone and its size band, and the large ones raise an alarm as they land.

Reads — a list of potentially damaging impacts and a map of where the floor takes them.

Used for — deciding where to inspect the floor at the next outage, and seeing whether a change in sootblowing has reduced the large impacts.

A bar chart of clinkers per blow for twelve sootblowers: six in the middle of the range, four with almost none, and two much higher and marked to run more next time.

Which sootblowers earn their steam

Each impact is counted against the sootblower that was running when the deposit let go. A sootblower that sheds a lot is working a fouled area; one that sheds nothing is blowing clean tubes.

Reads — clinkers per blow for every sootblower, and from that, where the superheater is fouling.

Used for — running the busy sootblowers more often and the idle ones less, by hand or through an intelligent sootblowing system.

A chart of impacts per hour through a chill-and-blow: the rate climbs to a peak in the first hour, falls away, and a vertical marker shows where shedding stopped.

When the chill-and-blow is done

During a chill-and-blow the boiler is off liquor while the deposits are cooled and blown. The app counts impacts per hour through the event, and shows the rate rise, peak and die away.

Reads — the shed rate now, and a flag when it has stayed below a set level.

Used for — ending the event when the shedding ends, and comparing one chill-and-blow with the last.

What goes on the boiler

CDS adds a small number of sensors under the floor and reads one signal the mill already has. Nothing is installed inside the furnace.

Floor accelerometers

Installed — industrial accelerometers on the floor’s supporting structure, under the boiler floor, wired to a stainless NEMA 4X enclosure.

Sees — every impact on the floor, with the zone it landed in.

Sootblower status

Installed — nothing new. ITM Connect reads which sootblower is running from the sootblower control system.

Used for — tying each impact to a sootblower and counting clinkers per blow.

ITM Connect at the edge

Installed — one ITM Compute unit for the boiler, running ITM Connect and the Clinker Detection App.

Used for — detecting and sizing impacts at the boiler, keeping the history, and sending results to the DCS, the sootblowing system and the historian.

Proven on a recovery boiler

CDS was developed with a major pulp and paper producer for a recovery boiler with a history of floor-tube damage, and was presented at the International Chemical Recovery Conference in 2017. The mill strengthened the floor-tube supports and installed CDS to see what was landing. A finite element model of the floor tubes, checked against the calibration drops, related clinker size to floor-tube deformation and gave that boiler its three size bands.

  • Large impacts were identified and traced to their source by matching them with sootblower operation.
  • During a chill-and-blow, most of the shedding came from two groups of sootblowers, and two sootblowers near the roof and front wall removed the most per run.
  • Four sootblowers shed very little, which showed where blowing was doing the least.
  • The impact count showed the shedding rise, peak and stop through the shutdown, in real time.
A trend of impacts per hour over three days on an operating recovery boiler, with six numbered events from the start of the shutdown to full operation; the count peaks at about 130 per hour as the boiler shuts down and falls to almost nothing before sootblowing stops.
Impacts per hour through a chill-and-blow on an operating recovery boiler
A table of twelve sootblowers with runs, impacts, weight in kilograms, impacts per run and weight per run; two sootblowers with nine runs each have the highest impacts and weight per run.
The same event, by sootblower: runs, impacts and equivalent weight

Why it matters

Sootblowers can take up to 6 percent of the steam a boiler generates, so a small cut in unnecessary blowing adds up over a year, and less steam used means less fuel burned for the same output. Blowing fouled areas more often keeps clinkers small, which lowers the risk to the floor. A chill-and-blow that ends when the shedding ends puts the boiler back on liquor sooner. The same measurement can also be used to judge sonic horns and pulse-detonation cleaning.

CDS is advisory. It measures what reaches the floor, not the deposits still on the tubes, and it reports an equivalent size, not a weight. Small debris below the recording threshold is not counted, and the char bed affects the reading. It does not detect a tube leak, it is not part of the boiler’s protection or trip system, and the sootblowing sequence remains the mill’s decision.

A typical deployment

  1. Survey the floor. With the boiler drawings, mark the supporting structure, agree the zones and choose the sensor positions.
  2. Install. Mount the accelerometers under the floor and run them to the enclosure.
  3. Connect the sootblower status. Read which sootblower is running from the sootblower control system.
  4. Calibrate. During an outage, drop known weights from the access ports onto the bare floor and record where each one lands.
  5. Set the bands. Agree what size of impact is a concern for this floor; a finite element study of the floor tubes can be added.
  6. Baseline. Run through several sootblowing cycles to see the normal number of impacts for each sootblower.
  7. Hand over to the control room. Agree how the large-impact alarm enters the DCS alarm list and who acts on it.
  8. Review. After the first weeks and the first chill-and-blow, review the sootblowing sequence against what each sootblower removed.
Side view of a recovery boiler’s upper furnace: superheater and generating bank tubes, numbered sootblower positions between them, the nose arch, and access holes below it with the note that the boiler floor is 30 meters below.
Sootblower positions, the nose arch and the access holes used for calibration

References: published sources behind this page.

Part of ITM’s patented boiler monitoring family installed worldwide.

Next step: pairs with ITM Connect CleanPass, which measures the deposits still on the tubes.

Talk to an engineer: (844) 837-8797 · info@iTestSystem.com

Related Edge Solutions resources